General Plywood - IS: 303

Veneers from high-quality logs are mechanically dried and they undergo a stress-relieving process, which is assembled in such a way, to form a balanced construction. High quality fortified synthetic resins are used for gluing the veneers. Glue line is poisoned by special formulations of chemicals to make Ogaan plywood safe against borers. It is hot pressed under proper temperature and more than then 16Kg/cm2 specific pressure. Conditioning is done after pressing, followed by preservative treatment.

Applications

MR grade is basically used for interior applications. BWR the grade is used in woodworking like ship cabins, Railway Coaches, Bus and Truck Bodies, Kitchen Cabinets, Exhaust pipes, False Ceilings, Speaker Cabinets, Bathroom Paneling etc.

Technical Specifications

Test Requirement of IS:303(BWR/MR) Test Result
Moisture Content Glue Adhesion 5-15% 6-10%
a)     Water Resistance Test Three cycles of 8 hours boiling in water and drying at 65±2°c For 16 hours, 3 hours at 60±2°c in water & drying 65±2°c for 8 hour Pass Standard
(b) Mycological test Static Bending Strength MOE (Modular of Elasticity) One cycle of 21 days Pass Standard
Along

Avg. N/mm2

Min. Ind. N/mm2

 

5000/4000

4500/3600

 

5500/4500

5000/4000

Across

Avg. N/mm2

Min. Ind. N/mm2

 

2500/2000

2200/1800

 

3000/2500

2500/2400

MOR (Modular of Rupture)

Along

Avg. N/mm2

Min. Ind. N/mm2

 

 

 

40/30

36/27

 

 

45/40

40/35

MOR (Modular of Rupture)

Along

Avg. N/mm2

Min. Ind. N/mm2

 

 

 

20/15

18/13

 

 

30/25

25/20